The Class J – Charpy and Izod Automatic Impact Testing System, when used to perform the Charpy Test on plastic pipes in accordance with the ISO 9854.1 standard, requires a specified velocity of striking of 3.8m/s. The striking velocity refers to the speed at which the pendulum impacts the plastic pipe specimen during the test. It is a crucial parameter that determines the energy transferred to the specimen and influences its fracture behaviour.
By complying with ISO 9854.1 standard and utilizing the Class J – Charpy and Izod Automatic Impact Testing System with the specified striking velocity of 3.8m/s, accurate and standardized testing can be conducted to evaluate the impact resistance and overall performance of plastic pipes. This information ensures a reliable and consistent assessment of plastic pipe materials in accordance with the specified test requirements.