The following are the energy levels for the Charpy and Izod tests in the Class J – Charpy and Izod Automatic Impact Testing System:
Charpy Test:
- 1 J: 0.5358983 Nm
- 2 J: 1.0717967 Nm
- 4 J: 2.1435935 Nm
- 5 J: 4.0192 Nm
- 15 J: 8.0385 Nm
- 25 J: 13.397 Nm
- 50 J: 26.795 Nm
Izod Test:
- 1 J: 0.5358983 Nm
- 75 J: 1.4737205 Nm
- 5 J: 2.94744 Nm
- 11 J: 5.8949 Nm
- 22 J: 11.7898 Nm
These energy levels indicate the amount of impact energy applied to specimens during testing. The values are measured in Newton-meters (Nm) and are crucial for assessing materials’ impact resistance and toughness. The Class J – Charpy and Izod Automatic Impact Testing System offers a range of energy levels to accommodate different testing requirements and ensure a comprehensive evaluation of material properties.