The following are the energy levels for the Charpy and Izod tests in the Class J – Charpy and Izod Automatic Impact Testing System:

Charpy Test:

  • 1 J: 0.5358983 Nm
  • 2 J: 1.0717967 Nm
  • 4 J: 2.1435935 Nm
  • 5 J: 4.0192 Nm
  • 15 J: 8.0385 Nm
  • 25 J: 13.397 Nm
  • 50 J: 26.795 Nm

Izod Test:

  • 1 J: 0.5358983 Nm
  • 75 J: 1.4737205 Nm
  • 5 J: 2.94744 Nm
  • 11 J: 5.8949 Nm
  • 22 J: 11.7898 Nm

These energy levels indicate the amount of impact energy applied to specimens during testing. The values are measured in Newton-meters (Nm) and are crucial for assessing materials’ impact resistance and toughness. The Class J – Charpy and Izod Automatic Impact Testing System offers a range of energy levels to accommodate different testing requirements and ensure a comprehensive evaluation of material properties.